Material Notes:
Description: Rhodasurf® L-4/STD is linear alcohol ethoxylate. It is oil in water emulsifier and stabilizer. It also exhibits dispersant and wetting properties.Chemical Name: LINEAR ALCOHOL ETHOXYLSATE C10-C16CAS: 68002-97-1Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODASURF© L-4/STD is a water in oil emulsifier used in honing oils, textile spin finishes and with anionics in emulsion polymerization. RHODASURF© L-4/STD is an APE-free nonionic emulsifier and stabilizer.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
pH 5.0 - 7.5
5.0 - 7.5
5% in 1/1 IPA/Water; RP-0420
Chemical Properties Metric English Comments
Total Acid Number <= 2.0
<= 2.0
[mg KOH/g]; RP-0008
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
@ 40°C, RP-0064
Clear to Cloudy Liquid
@ 25°C, RP-0064
Cloud Point <5°C
RP-123
Color <45
APHA, 50% in Ethanol, RP-0134
HLB number 9.7
Hydroxyl Number 148-154 mg KOH/g
RP-0245
Ionic Charge Nonionic
Moles of Ethylene Oxide 4