Material Notes:
Description: Rhodasurf® ON 870 is Ethoxylated Oleyl Alcohol. It is low foaming emulsifier. It is good wetting agent, dispersant, and detergent.Chemical Name: ETHOXYLATED OLEYL ALCOHOLCAS: 9004-98-2Available in: Asia Pacific, Europe, Latin America and North AmericaGel Test (50% Aqueous Solution): Immediately soluble @ 25°C, no gelling, RP-01289Applications: Rhodasurf ON-870® is used as low foaming emulsifier, wetting agent, dispersant and detergent in Bath products, Conditioners, Liquid Soap, Cleaners, Pretreatment & Plating formulations, Shampoo etc.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.03 - 1.04 g/cc
0.0372 - 0.0376 lb/in³
pH 6.0 - 8.0
6.0 - 8.0
0.1
Optical Properties Metric English Comments
Gardner Color Number <= 5.0
<= 5.0
Molten; RP-0138
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Karl Fisher; RP-0327
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance White to pale yellow soft wax
RP-0064
Neutralization Number <0.5 mg KOH/g
pH 7, RP-0343