Solvay RHODASURF® TR/15-40 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODASURF® TR/15-40 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Identification: WATER SOLUTION OF ETHOXYLATED TRIDECYL ALCOHOLCAS: 9043 – 30 – 5 ; 7732 – 18 – 5Solubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Emulsifier for industrial applicationsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
pH 5.0 - 7.0
5.0 - 7.0
5% in water; RPG02
Surface Tension 34 dynes/cm
34 dynes/cm
Thermal Properties Metric English Comments
Pour Point 13.0 °C
55.4 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
RPG31
Composition Active
0.4
Dry Substance
39-41%, RPG25
Critical Micelle Concentration 7E-05
Ionic Charge Nonionic
Moles of Ethylene Oxide 15