Solvay RHODICARE XC Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODICARE XC Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Rhodicare® XC is similar to standard Xanthan Gum, this grade displays improved microbial specifications. It has high electrolyte stability over a wide range of pH and fast hydration rate. It exhibits Pseudo-plastic non-thixotropic behaviour, antisyneresis agentand reduces gel exudation. Approved for Ecocert.C.T.F.A. /I.N.C.I. Name: XANTHAN GUMCAS: 11138 - 66 – 2EINECS: 234 – 394-2Recommended use level: 0.2 - 1%. Soluble in waterCompatible with Non-ionic, anionic and amphoteric surfactants.Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: Sodium salt of an anionic high molecular weight hetero-polysaccharide produced by pure culture fermentation of Xanthomonas campestris, purified by recovery with iso-propanol, dried and milled. Thickening and stabilizing hydrocolloid giving aqueous solutions of high viscosity and high yield value even at low concentrations, not affected by temperature. Pseudo-plastic non thixotropic behaviour. Effective suspending and stabilizing agent for multi-phasic systems: aqueous suspensions, emulsions and foams, easily sprayable, flowable, pumpable (creams and lotions, toothpastes…). Thickening agent for creams, suspensions, shampoos, gels; synergistic effect with galactomannanes, glucomannanes. Anti-syneresis agent, reduces gel exudation.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Bulk Density 0.700 - 0.800 g/cc
0.0253 - 0.0289 lb/in³
Particle Size 180 µm
180 µm
95 min, 80 mesh; TI-2087
250 µm
250 µm
99.5 min, 60 mesh; TI-2087
pH 6.0 - 8.0
6.0 - 8.0
1% aqueous sol.; TI-2076
Brookfield Viscosity 1200 - 1600 cP
1200 - 1600 cP
1% in 1% KCl; TI-1110
Descriptive Properties Value Comments
Appearance Fine powder
Assay 91-108%
TI-2091
Color Creamy white
Composition 2-Propanol
<750 ppm, TI-2105
Arsenic as As
<2 ppm, USP
Ash
6.5-16%, TI-0130
Entero-bacteria & other Gram Neg.
Absence in 1g, TI-2185
Esherichia coli
Absence in 5g, TI-2074
Heavy metal as Pb
<10 ppm, TI-2109
Lead as Pb
<2 mg/kg, USP
Pseudomonas aeruginosa
Absence in 1g, TI-2073
Salmonella species
Absence in 25g, TI-2074
Staphylococcus aureus
Absence in 1g, TI-2073
Total viable aerobic count
<500 cfu/g, TI-2070
Yeasts and moulds
<100 cfu/g, TI-2071