Solvay RHODOLINE® 646 Surfactant

Category Fluid
Manufacturer Solvay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODOLINE® 646 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Highly effective mineral oil defoamer for latex processing.Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© 646 may be post-added to a latex or coating color at a concentration of about 0.05 to 0.15%. For use in adhesives or paints, the suggested concentration is 2.5 to 5.0 pounds per 100 gallons of product. RHODOLINE© 646 may be stored over a wide range of temperatures. For ease of handling, storage above 40ºF is recommended. If the product should solidify due to cold, warm to room temperature and mix well before use.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.900 - 0.920 g/cc
0.0325 - 0.0332 lb/in³
RP-17617
pH 7.0 - 9.0
7.0 - 9.0
5% Solution; RP-0420
Viscosity 200 - 750 cP
200 - 750 cP
#2 SP @ 30 rpm; RP-0596
Ash 10 - 12 %
10 - 12 %
RP-0065
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Opaque, Gray Liquid
RP-0064
Hegman Test <6.0
Grind, RP-9186