Solvay SIPOMER® PAM-4000 Ethylmethacrylate Phosphate; Alkyl Methacrylate Phosphate

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name SIPOMER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay SIPOMER® PAM-4000 Ethylmethacrylate Phosphate; Alkyl Methacrylate Phosphate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Sipomer PAM-4000 incorporated into acrylic or styrene acrylic systems improves adhesion to metallic substrates. It also enhances properties such as polymer stability and gloss. This monomer has been used mainly in specialty purpose coatings, including industrial maintenance, OEM, as well as high performance structural adhesives.Chemical Name: ETHYLMETHACRYLATE PHOSPHATE; ALKYL METHACRYLATE PHOSPHATECAS: 52628-03-2, 7664-38-2, 868-77-9 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: SIPOMER ® PAM-4000 incorporated into acrylic or styrene acrylic systems improves adhesion to metallic substrates. It also enhances properties such as polymer stability and gloss. This monomer has been used mainly in specialty purpose coatings, including industrial maintenance, OEM, as well as high performance structural adhesives.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH <= 1.0
<= 1.0
Chemical Properties Metric English Comments
Total Acid Number 171 - 187
171 - 187
[mg KOH/g], #1; RP-0427
266 - 296
266 - 296
[mg KOH/g], #2; RP-0427
Processing Properties Metric English Comments
Moisture Content <= 0.25 %
<= 0.25 %
PRC11006
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Clear, Colorless to Pale Yellow Liquid
Color <300
APHA, RPC11004
Composition MEHQ
250-600 ppm, RP-1408
Phosphoric Acid
<4%, RP-0427
Odor Mild Acrylic Odor