Solvay SOPROPHOR® DSS/7 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name SOPROPHOR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay SOPROPHOR® DSS/7 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED ETHOXYLATED POLYARYLPHENOL SULPHATE, AMMONIUM SALTCAS: 59891 – 11 – 1Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North America Applications: Emulsifier, dispersing agentInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
pH 2.0 - 4.0
2.0 - 4.0
5% in water; RPG02
Thermal Properties Metric English Comments
Pour Point 22.0 °C
71.6 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
RPG16
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Viscous liquid
Composition Active
1
HLB number 13.5
Ionic Charge Anionic