Material Notes:
Description: Soprophor® S/25 is Tristyrylphenol ethoxylate, HLB = 14.5. It is nonionic multipurpose high performance emulsifier, soluble in water and most polar and aromatic solvents. Recommended as an alternative to alkoxylated nonylphenols. Gives high performance in preparation of micro-emulsionsIdentification: ETHOXYLATED TRISTYRYLPHENOLSolubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North America Applications: Emulsifiable Concentrates, Micro-emulsions, Emulsions in Water, Suspo-Emulsions, Suspension ConcentratesInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
pH 9.0 - 11
9.0 - 11
5% in water; RPG02
Thermal Properties Metric English Comments
Melting Point 35.0 °C
95.0 °F
Flash Point >= 100 °C
>= 212 °F
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
RPG16
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Solid
Composition Active
1
HLB number 14.9
Ionic Charge Nonionic