Solvay Specialty Polymers Ajediumâ„¢ Film Thermoplastic Polyimide (PI, TP)

Category Polymer , Film , Thermoplastic , Polyimide, Thermoplastic
Manufacturer Solvay Specialty Polymers
Trade Name Ajedium™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ajediumâ„¢ Film Thermoplastic Polyimide (PI, TP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPI is a thermoplastic polyimide film that has excellent, thermal, chemical, electrical and physical properties. With a continuous use temperature to 240°C (465°F), TPI films offer superior radiation resistance, excellent wear performance and resistance to chemicals.Features: Flame Retardant; Good Chemical Resistance; Good Electrical Properties; High Heat Resistance; Radiation (Gamma) ResistantUses: Aircraft Applications; Automotive Applications; Electrical/Electronic Applications; Industrial Applications; Medical/Healthcare Applications; Oil/Gas ApplicationsAdditional Properties: Area Factor - 145 ft²/lb/milInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ASTM D792
Water Absorption 1.0 %

@Time 86400 sec
1.0 %

@Time 24.0 hour
ISO 62
Thickness 100 microns
3.94 mil
As Tested
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 190 %
190 %
ASTM D882
Film Elongation at Yield, MD 7.0 %
7.0 %
ASTM D882
Secant Modulus, MD 3.05 GPa
442 ksi
ASTM D882
Dart Drop Test 400 g
0.882 lb
ASTM D1709
Film Tensile Strength at Break, MD 104 MPa
15100 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 388 °C
730 °F
ASTM D3418
Glass Transition Temp, Tg 250 °C
482 °F
DSC
Oxygen Index 47 %
47 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.5

@Frequency 1000 Hz
2.5

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 160 kV/mm

@Thickness 3.00 mm
4060 kV/in

@Thickness 0.118 in
ASTM D149
Dissipation Factor 0.0014

@Frequency 1000 Hz
0.0014

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
Latin America
North America
Color Orange
RoHS Compliance RoHS Compliant