Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Ajediumâ„¢ Films PPS Polyphenylene Sulfide (PPS)

Category Polymer , Film , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer Solvay Specialty Polymers
Trade Name Ajedium™ Films
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ajediumâ„¢ Films PPS Polyphenylene Sulfide (PPS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyphenylene sulfide, PPS, is a thermoplastic film that has excellent chemical resistance and good electrical and physical properties.Features: Flame Retardant; Good Chemical Resistance; Good Electrical Properties; Radiation (Gamma) ResistantUses: Aircraft Applications; Automotive Applications; Electrical/Electronic Applications; Industrial Applications; Oil/Gas ApplicationsAdditional Properties: Area Factor - 145 ft²/lb/milInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ISO 62
Thickness 75.0 microns
2.95 mil
As Tested
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 25 %
25 %
ASTM D882
Film Elongation at Yield, MD 3.5 %
3.5 %
ASTM D882
Secant Modulus, MD 2.37 GPa
344 ksi
ASTM D882
Dart Drop Test 0.600 g
0.00132 lb
ASTM D1709
Film Tensile Strength at Break, MD 46.9 MPa
6800 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 279 °C
534 °F
ASTM D3418
Glass Transition Temp, Tg 92.0 °C
198 °F
DSC
Oxygen Index 47 %
47 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+17 ohm-cm
1.50e+17 ohm-cm
ASTM D257
Dielectric Constant 3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 4.00 kV/mm

@Thickness 0.100 mm
102 kV/in

@Thickness 0.00394 in
ASTM D149
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
Latin America
North America
Color Yellow
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved