Solvay Specialty Polymers Algoflon® D 2510 F Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Solvay Specialty Polymers
Trade Name Algoflon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Algoflon® D 2510 F Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Algoflon® D 2510 F is a PFOA-free white aqueous PTFE dispersion. It is designed for impregnation processes and is particularly recommended for production of fabrics and laminates. Algoflon® D 2510 F exhibits excellent wetting properties and high shear stability. Algoflon® D 2510 F has low foaming behavior and is optimized for basecoat passes.Features: Good Chemical Resistance; High Heat Resistance; Low FrictionUses: Coating Applications; Impregnation ApplicationsAdditional Properties: Average Particle Size - Internal Method 0.24 µm; Brookfield Viscosity - 25 mPa·s; Density - ASTM D4441 1.51 g/m³; Non Ionic Surfactant - ASTM D4441 3.0 wt%; pH - ASTM D4441 > 9.0; PTFE Content - ASTM D4441 60.0 wt%Information provided by Solvay Specialty Polymers.
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color White
Form Latex