Solvay Specialty Polymers Algoflon® L101 Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Solvay Specialty Polymers
Trade Name Algoflon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Algoflon® L101 Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Algoflon® L101 a white PTFE micronized powder produced from dispersion polymerization comprising loose agglomerates of sub-micron sized primary particles. Algoflon® L101 can be de-agglomerated to sub-micron particle size by the application of shear providing a better dispersion and distribution of the PTFE particles in the application. Designed for use in critical engineering and high end performance lubricants, Algoflon® L101 will improved thickening effect, lubricity, improved corrosion and temperature resistance.Additional Properties: Average Particle Size - Internal Method 3.5 µm; Bulk Density - ASTM D4895 325 g/l; Specific Surface Area - Internal Method > 14 m²/gInformation provided by Solvay Specialty Polymers.
Thermal Properties Metric English Comments
Melting Point 325 - 335 °C
617 - 635 °F
ASTM D3418
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color White
Form Powder