Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.125 inch (3 mm).Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; Heat Stabilized; High Heat Resistance; High Strength; Low Moisture AbsorptionUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; Fuel Lines; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Thick-walled Parts; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D4000 PA121 G45 Color: BK324 Black; ASTM D4000 PA121 G45 Color: NT Natural; ASTM D5336 PPA0120 G45 A06637 Color: BK324 Black; ASTM D6779 PA121G45; BOSCH N28 BN05-OX1 BN0510-GF45-3Anf10SO Color: NT Natural; BOSCH N28 BN05-OX1 BN0510-GF45-3Asw01SO Color: BK324 Black; DELPHI DCM4889 Color: BK324 Black; DELPHI DCM4889 Color: NT Natural; DELPHI M-6073 Color: BK324 Black; FORD WSK-M4D861-A2 Color: BK324 Black; FORD WSK-M4D861-A2 Color: NT Natural; ISO 1874 PA6T/6I/66, MH, 12-160, GF45 Color: BK324 Black; ISO 1874 PA6T/6I/66, MH, 12-160, GF45 Color: NT Natural; VALEO VMS-8108 Color: BK324 BlackInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ISO 1183
Filler Content 45 %
45 %
Glass Fiber
Water Absorption 0.12 %

@Time 86400 sec
0.12 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 125
125
ASTM D785
Tensile Strength at Break 259 MPa
37600 psi
ASTM D638
263 MPa
38100 psi
ISO 527-2
Elongation at Break 2.6 %
2.6 %
ASTM D638
2.7 %
2.7 %
ISO 527-2
Tensile Modulus 16.0 GPa
2320 ksi
ISO 527-2
17.2 GPa
2490 ksi
ASTM D638
Flexural Strength 376 MPa
54500 psi
ISO 178
Flexural Yield Strength 363 MPa
52600 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
14.8 GPa
2150 ksi
ISO 178
Compressive Strength 314 MPa
45500 psi
ASTM D695
Poissons Ratio 0.41
0.41
ASTM E132
Shear Strength 108 MPa
15700 psi
ASTM D732
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
Izod Impact, Unnotched 13.0 J/cm
24.4 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
Type 1, Notch A; ISO 180
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
Type 1, Edgewise; ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 11.0 µm/m-°C

@Temperature 160 - 250 °C
6.11 µin/in-°F

@Temperature 320 - 482 °F
2
14.0 µm/m-°C

@Temperature 0.000 - 100 °C
7.78 µin/in-°F

@Temperature 32.0 - 212 °F
2
CTE, linear, Transverse to Flow 50.0 µm/m-°C

@Temperature 0.000 - 100 °C
27.8 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
100 µm/m-°C

@Temperature 100 - 250 °C
55.6 µin/in-°F

@Temperature 212 - 482 °F
TMA; ASTM E831
Melting Point 312 °C
594 °F
ASTM D3418
312 °C
594 °F
ISO 11357-3
Maximum Service Temperature, Air 165 - 185 °C
329 - 365 °F
Continuous Use
Deflection Temperature at 0.46 MPa (66 psi) 301 °C

@Thickness 3.20 mm
574 °F

@Thickness 0.126 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 279 °C
534 °F
Unannealed; ISO 75-2/A
287 °C

@Thickness 3.20 mm
549 °F

@Thickness 0.126 in
Annealed; ASTM D648
Flammability, UL94 HB

@Thickness 3.18 mm
HB

@Thickness 0.125 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 4.4

@Frequency 1.00e+6 Hz
4.4

@Frequency 1.00e+6 Hz
ASTM D150
4.6

@Frequency 60.0 Hz
4.6

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149
Dissipation Factor 0.0050

@Frequency 60.0 Hz
0.0050

@Frequency 60.0 Hz
ASTM D150
0.016

@Frequency 1.00e+6 Hz
0.016

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 145 sec
145 sec
ASTM D495
Comparative Tracking Index 550 V
550 V
UL 746
Processing Properties Metric English Comments
Processing Temperature 79.4 °C
175 °F
Hopper
Rear Barrel Temperature 304 - 318 °C
579 - 604 °F
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 135 °C
275 °F
Drying Temperature 121 °C

@Time 14400 sec
250 °F

@Time 4.00 hour
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant