Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically to be cost effective for most applications requiring high stiffness, good dimensional stability and chemical resistance.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Toughness; Heat Stabilized; High Heat Resistance; High Strength; Low CLTE; Ultra High StiffnessUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Thick-walled Parts; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D6779 PA122R65 Color: BK324 Black; ASTM D6779 PA122R65 Color: BK545 Black; ASTM D6779 PA122R65 Color: NT Natural; BMW GS 93016; DELPHI DCM4899 Color: BK324 Black; DELPHI DCM4899 Color: NT Natural; DELPHI M-2987 Color: BK324 Black; DELPHI M-2987 Color: NT Natural; DELPHI M-53292; DELPHI M-53292 Color: BK545 Black; GM GM7001M PA6T/6I/66 A3 A22 A42 A64 BJ721 DE1830 KS1750 Color: NT Natural; GM GMP.PPA.003 Color: Black; GM GMP.PPA.003 Color: Natural; GM GMW16358P-PPA-GF43MD22 Color: BK324 Black; GM GMW16358P-PPA-GF43MD22 Color: NT Natural; ISO 1874 PA6T/6I/66, MH, 11-120, (GF+MD)64 Color: BK324 Black; ISO 1874 PA6T/6I/66, MH, 11-120, (GF+MD)64 Color: NT Natural; TRW SP-13161601 Color: BK324 Black; TRW SP-13161601 Color: NT NaturalInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.84 g/cc
0.0665 lb/in³
Dry; ISO 1183
Filler Content 65 %
65 %
GlassMineral
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
Dry
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Dry; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 175 MPa
25400 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Tensile Modulus 20.9 GPa
3030 ksi
ASTM D638
Flexural Strength 263 MPa
38100 psi
ASTM D790
Flexural Modulus 19.9 GPa
2890 ksi
ASTM D790
Shear Strength 62.7 MPa
9090 psi
ASTM D732
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 311 °C
592 °F
Peak; Dry; ASTM D3418
311 °C
592 °F
Dry; ISO 11357-3
Processing Properties Metric English Comments
Processing Temperature 79.4 °C
175 °F
Hopper
Rear Barrel Temperature 307 - 329 °C
585 - 624 °F
Front Barrel Temperature 307 - 329 °C
585 - 624 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 65.6 - 166 °C
150 - 331 °F
Drying Temperature 120 °C

@Time 14400 sec
248 °F

@Time 4.00 hour
Moisture Content <= 0.045 %
<= 0.045 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant