Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Conditioned  (discontinued **)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Conditioned  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Asia Pacific; Europe; North AmericaInformation provide by Solvay Specialty Polymers
Mechanical Properties Metric English Comments
Tensile Strength 172 MPa
24900 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Tensile Modulus 11.7 GPa
1700 ksi
ASTM D638
Flexural Strength 241 MPa
35000 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Compressive Strength 172 MPa
24900 psi
ASTM D695
Shear Strength 75.8 MPa
11000 psi
ASTM D732
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+14 ohm-cm
5.00e+14 ohm-cm
ASTM D257
Dielectric Constant 3.4

@Frequency 1.00e+6 Hz
3.4

@Frequency 1.00e+6 Hz
ASTM D150
4.3

@Frequency 60.0 Hz
4.3

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm

@Thickness 1.60 mm
508 kV/in

@Thickness 0.0630 in
ASTM D149
Dissipation Factor 0.019

@Frequency 1.00e+6 Hz
0.019

@Frequency 1.00e+6 Hz
ASTM D150
0.020

@Frequency 60.0 Hz
0.020

@Frequency 60.0 Hz
ASTM D150
Comparative Tracking Index 600 V
600 V
High Voltage Arc-Tracking Rate, HVTR 18.0 mm/min
0.709 in/min
UL 746