Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better mechanical properties than many unreinforced thermoplastic polyester and nylon resins. Features: Ductile; Good Chemical Resistance; Heat Stabilized; Hot Water Moldability; Impact Modified; Low Temperature Impact Resistance; Low Warpage; LubricatedUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Machine/Mechanical Parts; Metal Replacement; Valves/Valve PartsInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications DELPHI M-4853 Color: BK718 Black; DELPHI MS008756 Color: NT Natural; DELPHI MS008759 Color: BK718 Black; FORD WSS-M4D1008-A1; GM GMP.PPA.015 Color: Black; GM GMP.PPA.015 Color: Natural; GM GMW16799P-PPA Color: Natural; IMDS ID 11974222 Color: Black; IMDS ID 11974222 Color: NaturalInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Dry; ISO 1183
Linear Mold Shrinkage, Flow 0.020 cm/cm
0.020 in/in
Dry
Linear Mold Shrinkage, Transverse 0.021 cm/cm
0.021 in/in
Dry; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 76.5 MPa
11100 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D638
Flexural Strength 73.1 MPa
10600 psi
ASTM D790
Flexural Modulus 2.28 GPa
331 ksi
ASTM D790
Shear Strength 57.2 MPa
8300 psi
ASTM D732
Izod Impact, Notched 1.50 J/cm
2.81 ft-lb/in
ASTM D256
Dart Drop, Total Energy 47.5 J
35.0 ft-lb
Instrumented; ASTM D3763
Thermal Properties Metric English Comments
Melting Point 315 °C
599 °F
Peak; Dry; ASTM D3418
315 °C
599 °F
Dry; ISO 11357-3
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+14 ohm-cm
7.00e+14 ohm-cm
ASTM D257
Surface Resistance 2.50e+13 ohm
2.50e+13 ohm
ASTM D257
Dielectric Constant 3.8

@Frequency 60.0 Hz
3.8

@Frequency 60.0 Hz
ASTM D150
3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Dissipation Factor 0.018

@Frequency 60.0 Hz
0.018

@Frequency 60.0 Hz
ASTM D150
0.035

@Frequency 1.00e+6 Hz
0.035

@Frequency 1.00e+6 Hz
ASTM D150
Comparative Tracking Index >= 600 V
>= 600 V
ASTM D3638
High Voltage Arc-Tracking Rate, HVTR 12.0 mm/min
0.472 in/min
UL 746
Processing Properties Metric English Comments
Rear Barrel Temperature 304 °C
579 °F
Front Barrel Temperature 324 °C
615 °F
Melt Temperature 321 - 329 °C
610 - 624 °F
Mold Temperature <= 90.0 °C
<= 194 °F
Drying Temperature 110 °C

@Time 14400 sec
230 °F

@Time 4.00 hour
Moisture Content <= 0.060 %
<= 0.060 %
Screw Speed 100 - 200 rpm
100 - 200 rpm
Descriptive Properties Value Comments
Additive Heat Stabilizer
Impact Modifier
Lubricant
Mold Release
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Processing Technique Water-Heated Mold Injection Molding
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.5:1.0