Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Conditioned)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 20% Glass Fiber Reinforced
Manufacturer Solvay Specialty Polymers
Trade Name Amodel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stability, chemical resistance and ductility. This resin has a high heat deflection temperature and a high flexural modulus, with greater tensile elongation than untoughened glass reinforced PPA.Features: Good Chemical Resistance; Good Dimensional Stability; Heat Stabilized; High Heat Resistance; Impact ModifiedUses: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Bearings; Bobbins; Connectors; General Purpose; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal ReplacementInjection Molding Notes: Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.Automotive Specifications ASTM D4000 PPA0111 G17 KD124 KN055 PN046 YI238 LD002 Color: BK 324 Black; ASTM D4000 PPA0111 G17 KD124 KN055 PN046 YI238 LD002 Color: NT Natural; ASTM D6779 PA123G15 YI220; GM GMN6828 Color: BK 324 Black; GM GMN6828 Color: NT Natural; GM GMP.PPA.009 Color: BK 324 Black; GM GMP.PPA.009 Color: NT Natural; GM GMW15702-021991 Color: BK 324 Black; GM GMW15702-021991 Color: NT Natural; GM GMW16359P-PPA-GF15 Color: BK 324 Black; GM GMW16359P-PPA-GF15 Color: NT Natural; ISO 1874-PA 6T/6I/66-HI, MH, 12-060, GF16; YAZAKI YPES-25-02-305 Color: BK 324 Black; YAZAKI YPES-25-02-305 Color: NT NaturalInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
Dry; ISO 1183
Filler Content 16 %
16 %
Glass Fiber
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Dry
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Dry; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 131 MPa
19000 psi
ASTM D638
Elongation at Break 2.8 %
2.8 %
ASTM D638
Tensile Modulus 7.10 GPa
1030 ksi
ASTM D638
Flexural Strength 201 MPa
29200 psi
ASTM D790
Flexural Modulus 6.21 GPa
901 ksi
ASTM D790
Shear Strength 65.5 MPa
9500 psi
ASTM D732
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.00 J/cm
15.0 ft-lb/in
ASTM D256
Dart Drop, Total Energy 7.59 J
5.60 ft-lb
Instrumented; ASTM D3763
Thermal Properties Metric English Comments
Melting Point 310 °C
590 °F
Peak; Dry; ASTM D3418
Processing Properties Metric English Comments
Rear Barrel Temperature 304 - 318 °C
579 - 604 °F
Front Barrel Temperature 316 - 329 °C
601 - 624 °F
Melt Temperature 321 - 343 °C
610 - 649 °F
Mold Temperature 135 °C
275 °F
Drying Temperature 110 °C

@Time 14400 sec
230 °F

@Time 4.00 hour
Moisture Content <= 0.045 %
<= 0.045 %
Descriptive Properties Value Comments
Additive Heat Stabilizer
Impact Modifier
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Natural
Form Pellets
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant