Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH  (discontinued **)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properties than many unreinforced thermoplastic polyester and nylon resins especially after exposure to humid environments. These materials were specifically designed for automotive electrical and electronic applications such as connectors, sockets, and sensors. Additional applications include fuel systems where both the high elongation/ductility and superior low permeation performance to automotive fuels are needed. They can be processed readily using conventional injection molding equipment and methods.Information provided by Solvay Advanced Polymers
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.50 %
0.50 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.019 cm/cm
0.019 in/in
93°C; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Elongation at Yield 50 %
50 %
ASTM D638
Tensile Modulus 2.50 GPa
363 ksi
ASTM D638
Flexural Strength 71.0 MPa
10300 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Shear Strength 47.0 MPa
6820 psi
ASTM D732
Izod Impact, Notched 8.00 J/cm
15.0 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
Dynatup @ -18°C 47.0 J
34.7 ft-lb
Total Energy. 50% RH. No temperature indicated.; D3763
Dynatup @ -18°C Max Load 408000 g
900 lb
No temperature indicated.; D3763
Thermal Properties Metric English Comments
Melting Point 300 °C
572 °F
ASTM D3418
Shrinkage 2.0 %
2.0 %
Electrical Properties Metric English Comments
Volume Resistivity 2.50e+15 ohm-cm
2.50e+15 ohm-cm
ASTM D257
Surface Resistance 2.50e+15 ohm
2.50e+15 ohm
ASTM D257
Dielectric Constant 3.6

@Frequency 60 Hz
3.6

@Frequency 60 Hz
ASTM D150
3.6

@Frequency 1e+6 Hz
3.6

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Dissipation Factor 0.012

@Frequency 60 Hz
0.012

@Frequency 60 Hz
ASTM D150
0.027

@Frequency 1e+6 Hz
0.027

@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index >= 600 V
>= 600 V
ASTM D3638
High Voltage Arc-Tracking Rate, HVTR 8.80 mm/min
0.346 in/min
UL 746A