Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Diofan® A 036 Polyvinylidene Chloride (PVDC)  (discontinued **)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Diofan® A 036 Polyvinylidene Chloride (PVDC)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DIOFAN® A 036 is a PVDC latex used as a flexible under layer for coating on paper and cardboard, to be covered with an appropriate topcoat.Additional Information: PROCESSING - DRYING - DIOFAN® A 036 coatings, being flexible under layers, should be covered by a topcoat such as DIOFAN® A 050, which has a lower surface tension. Reverse gravure roll and air knife are suitable coating techniques. - A good quality coating requires adequate drying, since higher temperatures will result in better barrier properties. FOOD AND DRUG LEGISLATION - The monomers used for the production of DIOFAN® A 036 comply with the requirements of the EU Commission Regulation No 10/2011 of 14 January 2011. - All the components are listed in the European Resolution AP 2004 (1) (Surface coating intended to come into contact with foodstuffs). - DIOFAN® A 036 complies with U.S. FDA chapters 21 CFR 175.320, 176.170 and 176.180. - The monomers used for the production of DIOFAN® A 036 comply with the Regulation (EC) 1907/2006 of the European Parliament and of the Council of 18 December 2006 concerning the Registration, Evaluation, Authorization and Restriction of Chemicals (REACH). - SolVin will provide necessary certification upon request by its customers. ISO CERTIFICATION - The implemented management system for the production, internal transfer and delivery, design and development of DIOFAN vinylidene chloride copolymers (PVDC) produced in Tavaux has been assessed and found to meet the requirements of ISO 9001: 2008, ISO 14001: 2004 and OHSAS 18001: 2007.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
1.65 g/cc
0.0596 lb/in³
Coating on BOPP
Solids Content 55 %
55 %
pH 3.0
3.0
Water Vapor Transmission 28.0 g/m²/day

@Temperature 38.0 °C
1.80 g/100 in²/day

@Temperature 100 °F
90% RH; 1 µm Coating on BOPP
Oxygen Transmission Rate 80.0 cc/m²/day
5.15 cc/100 in²/day
25°C, 1.0 µm, 85% RH; Coating on BOPP
Viscosity 25 cP

@Temperature 20.0 °C
25 cP

@Temperature 68.0 °F
Surface Tension 37 dynes/cm
37 dynes/cm
Foaming tendency
Mechanical Properties Metric English Comments
Coefficient of Friction, Dynamic <= 0.30
<= 0.30
vs. Itself - Coating on BOPP
Heat Seal Strength Initiation Temperature <= 100 °C
<= 212 °F
Heat Seal Threshold; 0.4 N/cm; Coating on BOPP
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month
23°C
Descriptive Properties Value Comments
Agency Ratings EC 1907/2006 (REACH)
EU No 10/2011
FDA 21 CFR 175.320
FDA 21 CFR 176.170
FDA 21 CFR 176.180
Availability Asia Pacific
Europe
North America
Emulsion Type Anionic
Features Good Flexibility
Filmability 14°C
Minimum Film Forming Temperature
Forms Liquid
Generic PVDC
Heat Seal Maximum Resistance > 2.0 N/cm
Coating on BOPP
Uses Coating Applications
Users viewing this material also viewed the following: