Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Diofan® A 050 Polyvinylidene Chloride (PVDC)  (Unverified Data**)

Category Polymer , Thermoplastic , PVDC , Polyvinyl Dichloride (PVDC)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Diofan® A 050 Polyvinylidene Chloride (PVDC)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DIOFAN® A 050 is a standard grade PVDC latex for coating on various substrates. It is generally used as a topcoat on paper, cardboard and as a coating on plastic films.Additional Information: PROCESSING - DRYING - DIOFAN® A 050 exhibits excellent mechanical stability that allows it to be processed with different coating techniques, Including reverse gravure roll and air knife coating systems. - When coating plastic films, DIOFAN® A 050 should be formulated with wax and silica in order to improve the blocking and slip properties of the finished coating. - A good quality coating requires adequate drying, since higher temperatures will result in better barrier properties. FOOD AND DRUG LEGISLATION - The monomers used for the production of DIOFAN® A 050 comply with the requirements of the EU Commission Regulation No 10/2011 of 14 January 2011. - All the components are listed in the European Resolution AP 2004 (1) (Surface coating intended to come into contact with foodstuffs). - DIOFAN® A 050 complies with U.S. FDA chapters 21 CFR 175.105, 175.300, 176.170, 176.180 and 177.1630. - The monomers used for the production of DIOFAN® A050 comply with the Regulation (EC) 1907/2006 of the European Parliament and of the Council of 18 December 2006 concerning the Registration, Evaluation, Authorization and Restriction of Chemicals (REACH). - SolVin will provide necessary certification upon request by its customers. ISO CERTIFICATION - The implemented management system for the production, internal transfer and delivery, design and development of DIOFAN vinylidene chloride copolymers (PVDC) produced in Tavaux has been assessed and found to meet the requirements of ISO 9001: 2008, ISO 14001: 2004 and OHSAS 18001: 2007.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.300 g/cc
0.04697 lb/in³
1.650 g/cc
0.05961 lb/in³
Coating on BOPP
Solids Content 58 %
58 %
pH 3.0
3.0
Water Vapor Transmission 16.0 g/m²/day

@Temperature 38.0 °C
1.03 g/100 in²/day

@Temperature 100 °F
90% RH; 1 µm Coating on BOPP
Oxygen Transmission Rate 54.0 cc/m²/day
3.48 cc/100 in²/day
25°C, 1.0 µm, 85% RH; Coating on BOPP
Viscosity 10 cP

@Temperature 20.0 °C
10 cP

@Temperature 68.0 °F
Surface Tension 32 dynes/cm
32 dynes/cm
Foaming tendency
Mechanical Properties Metric English Comments
Coefficient of Friction, Dynamic 0.21
0.21
vs. Itself - Coating on BOPP
Heat Seal Strength Initiation Temperature 111 °C
232 °F
Heat Seal Threshold; 0.4 N/cm; Coating on BOPP
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
23°C
Descriptive Properties Value Comments
Agency Ratings EC 1907/2006 (REACH)
EU No 10/2011
FDA 21 CFR 175.105
FDA 21 CFR 175.300
FDA 21 CFR 176.170
FDA 21 CFR 176.180
FDA 21 CFR 177.1630
Availability Asia Pacific
Europe
North America
Emulsion Type Anionic
Filmability 18°C
Minimum Film Forming Temperature
Forms Liquid
Generic PVDC
Heat Seal Maximum Resistance 2.3 N/cm
Coating on BOPP
Uses Coating Applications