Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Hyflon® AD 40H Perfluoropolymer

Category Polymer , Thermoplastic , Fluoropolymer , TFE/Perfluoromethylvinylether Copolymer (MFA)
Manufacturer Solvay Specialty Polymers
Trade Name Hyflon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Hyflon® AD 40H Perfluoropolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hyflon® AD 40H is an amorphous perfluoro-polymer available in powder form. Hyflon® AD polymers resemble semicrystalline perfluoropolymers in their performance properties as they exhibit high temperature stability, excellent hydrophobicity and chemical resistance as well as very low surface energy. Key distinctive feature of Hyflon AD polymers is that they are soluble in selected solvents. In particular, their high solubility in perfluorinated solvents and their low solution viscosities make them suitable for solution process technologies.Hyflon® AD can provide uniform and thin films or coatings (down to submicron thicknesses if required) by casting or coating techniques and thermal treatments, well below the typical baking temperatures of semicrystalline perfluoro-polymers.Features: Amorphous; Good Chemical Resistance; Good Thermal StabilityUses: Coating Applications; FilmAdditional Properties: Intrinsic Viscosity - ASTM D2857 (30°C): 1.3 dl/gInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.98 g/cc
0.0715 lb/in³
ASTM D792
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 90.0 °C
194 °F
ASTM E1356
Optical Properties Metric English Comments
Refractive Index 1.331
1.331
ASTM D542
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Form Powder
Processing Technique Coating; Solution Processing
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved