Solvay Specialty Polymers Hyflon® PFA C920-0020X Perfluoroalkoxy (PFA)

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer Solvay Specialty Polymers
Trade Name Hyflon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Hyflon® PFA C920-0020X Perfluoroalkoxy (PFA).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hyflon® PFA C920-0020X is a semi crystalline, melt processable perfluoroalkoxy fluorocarbon resin specifically designed for applications where the unique properties of PFAs must be combined with antistatic performance.Hyflon® PFA C920-0020X is a low melt flow rate multi-purpose resin designed for pipe and stock shapes extrusion, compression, and transfer molding. Thanks to its low melting point, the C920-0020X offers inherent lower processing costs and can be used in a wider range of processing conditions.Additional Properties: Melt Flow - ASTM D1238 1.50 to 7.50 g/10 minInformation provided by Solvay Specialty Polymers.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 22.0 MPa
>= 3190 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 255 - 270 °C
491 - 518 °F
DSC
Electrical Properties Metric English Comments
Volume Resistivity 1000 - 1.00e+8 ohm-cm
1000 - 1.00e+8 ohm-cm
ASTM D257
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Form Pellets
Processing Technique Compression Molding; Extrusion; Resin Transfer Molding