Solvay Specialty Polymers Kadel® E-1130 Polyketone  (discontinued **)

Category Polymer , Thermoplastic , Polyketone
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Kadel® E-1130 Polyketone  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical resistance for application in hostile environments.This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
in 24 hours per ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 163 MPa
23600 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Tensile Modulus 9.72 GPa
1410 ksi
ASTM D638
Flexural Yield Strength 235 MPa
34100 psi
ASTM D790
Flexural Modulus 10.0 GPa
1450 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Tensile Impact Strength 140 kJ/m²
66.6 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 20.0 °C
10.6 µin/in-°F

@Temperature 68.0 °F
ASTM E381
Deflection Temperature at 1.8 MPa (264 psi) 326 °C
619 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.60e+18 ohm-cm
1.60e+18 ohm-cm
ASTM D257
Dielectric Constant 3.7

@Frequency 1000 Hz
3.7

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm

@Thickness 0.320 mm
381 kV/in

@Thickness 0.0126 in
ASTM D149
Users viewing this material also viewed the following: