Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KetaSpire KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughness-related properties, such as impact resistance and elongation at break. The low fiberglass loading gives the resin improved surface aesthetics and reduced anisotropy over comparable 30% glass reinforced formulations. KetaSpire PEEK is produced to the highest industry standards and is characterized by a distinct combination of best-in-class fatigue resistance, ease of melt processing, high purity, and excellent chemical resistance to organics, acids, and bases. These properties make it well-suited for applications in oil and gas recovery, semiconductor fabrication, automotive, aerospace, healthcare, chemical processing, and other industrial uses. This resin is opaque and beige to light brown in color in its natural state. - Beige: KT-820 GF13 BG20Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Filler Content 13 %
13 %
Glass Fiber Reinforcement
Viscosity 534000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
534000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; Internal Method
Mechanical Properties Metric English Comments
Tensile Strength 117 MPa
17000 psi
ASTM D638
Elongation at Break 6.2 %
6.2 %
ASTM D638
Elongation at Yield 3.9 %
3.9 %
ASTM D638
Tensile Modulus 5.90 GPa
856 ksi
ASTM D638
Flexural Strength 203 MPa
29400 psi
ASTM D790
Flexural Modulus 5.60 GPa
812 ksi
ASTM D790
Izod Impact, Notched 0.910 J/cm
1.70 ft-lb/in
ASTM D256
10.0 J/cm
18.7 ft-lb/in
ASTM D4218
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 213 °C
415 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 365 °C
689 °F
Middle Barrel Temperature 370 °C
698 °F
Front Barrel Temperature 375 °C
707 °F
Nozzle Temperature 380 °C
716 °F
Mold Temperature 175 - 205 °C
347 - 401 °F
Drying Temperature 150 °C
302 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Appearance Beige
Opaque
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Fatigue Resistant
Flame Retardant
Good Chemical Resistance
Good Dimensional Stability
High Heat Resistance
High Stiffness
High Strength
Forms Pellets
Powder
Generic PEEK
Injection Rate Fast
Processing Method Injection Molding
Machining
Profile Extrusion
Screw Compression Ratio 2.5:1.0 to 3.5:1.0
Uses Industrial Applications
Medical/Healthcare Applications
Oil/Gas Applications