Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire PEEK resin. Reinforcement also affords greater mechanical robustness in structural applications, particularly those with service temperatures approaching 300°C. KetaSpire PEEK is produced to the highest industry standards and is characterized by a distinct combination of best-in-class fatigue resistance, ease of melt processing, high purity, and excellent chemical resistance to organics, acids, and bases. These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing, and other industrial uses. Beige: KetaSpire KT-820 GF30 BG20Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc
1.53 g/cc
ASTM D792
Filler Content 30 %
30 %
Glass Fiber Reinforcement
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Viscosity 850000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
850000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Thickness 3.18 mm
0.0020 - 0.0040 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125"; ASTM D955
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm

@Thickness 3.18 mm
0.014 - 0.016 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125"; ASTM D955
Melt Flow 0.70 g/10 min

@Load 2.16 kg,
Temperature 400 °C
0.70 g/10 min

@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 100
100
M-Scale; ASTM D785
Hardness, Shore D 91

@Time 1.00 sec
91

@Time 0.000278 hour
ASTM D2240
Tensile Strength 158 MPa
22900 psi
ASTM D638
Tensile Strength, Yield 158 MPa
22900 psi
5.0 mm/min; ASTM D638
165 MPa
23900 psi
ISO 527-2/1A/5
Elongation at Break 2.7 %
2.7 %
5.0 mm/min; ASTM D638
2.7 %
2.7 %
ISO 527-2/1A/5
Tensile Modulus 10.5 GPa
1520 ksi
5.0 mm/min; ASTM D638
11.4 GPa
1650 ksi
ISO 527-2/1A/1
Flexural Strength 246 MPa
35700 psi
ISO 178
261 MPa
37900 psi
ASTM D790
Flexural Yield Strength 261 MPa
37900 psi
ASTM D790
Flexural Modulus 10.4 GPa
1510 ksi
ASTM D790
10.7 GPa
1550 ksi
ISO 178
Compressive Strength 169 MPa
24500 psi
ASTM D695
Poissons Ratio 0.34
0.34
ASTM E132
Shear Modulus 3.92 - 4.25 GPa
569 - 616 ksi
Calculated
Shear Strength 93.1 MPa
13500 psi
ASTM D732
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
9.60 J/cm
18.0 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) 56.0 kJ/m²
26.6 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
9.44 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
Specific Heat Capacity 1.30 J/g-°C

@Temperature 50.0 °C
0.311 BTU/lb-°F

@Temperature 122 °F
DSC
1.73 J/g-°C

@Temperature 200 °C
0.413 BTU/lb-°F

@Temperature 392 °F
DSC
Thermal Conductivity 0.290 W/m-K
2.01 BTU-in/hr-ft²-°F
ASTM E1530
Melting Point 340 °C
644 °F
Peak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 315 °C
599 °F
Annealed; ASTM D648
Glass Transition Temp, Tg 150 °C
302 °F
ASTM D3418
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
UL 94
V-0

@Thickness 20.3 mm
V-0

@Thickness 0.799 in
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+17 ohm-cm
1.90e+17 ohm-cm
ASTM D257
Surface Resistance >= 1.90e+17 ohm
>= 1.90e+17 ohm
ASTM D257
Dielectric Constant 3.41

@Frequency 1.00e+6 Hz
3.41

@Frequency 1.00e+6 Hz
ASTM D150
3.44

@Frequency 1000 Hz
3.44

@Frequency 1000 Hz
ASTM D150
3.44

@Frequency 60.0 Hz
3.44

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm

@Thickness 3.00 mm
432 kV/in

@Thickness 0.118 in
ASTM D149
Dissipation Factor 0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
ASTM D150
0.0010

@Frequency 60.0 Hz
0.0010

@Frequency 60.0 Hz
ASTM D150
0.0030

@Frequency 1.00e+6 Hz
0.0030

@Frequency 1.00e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Rear Barrel Temperature 365 °C
689 °F
Middle Barrel Temperature 370 °C
698 °F
Front Barrel Temperature 375 °C
707 °F
Nozzle Temperature 380 °C
716 °F
Mold Temperature 175 - 205 °C
347 - 401 °F
Drying Temperature 150 °C
302 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Agency Ratings ISO 10993
ISO 10993-Part 1
Appearance Beige
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Autoclave Sterilizable
E-beam Sterilizable
Ethylene Oxide Sterilizable
Fatigue Resistant
Flame Retardant
Good Chemical Resistance
Good Dimensional Stability
Good Sterilizability
Heat Sterilizable
High Heat Resistance
High Stiffness
High Strength
Radiation (Gamma) Resistant
Radiation Sterilizable
Radiotranslucent
Steam Resistant
Steam Sterilizable
Forms Pellets
Powder
Generic PEEK
Injection Rate Fast
Processing Method Injection Molding
Machining
Profile Extrusion
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.5:1.0 to 3.5:1.0
Uses Aircraft Applications
Connectors
Dental Applications
Electrical/Electronic Applications
Film
Hospital Goods
Industrial Applications
Medical Appliances
Medical/Healthcare Applications
Oil/Gas Applications
Seals
Surgical Instruments
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved