Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Solvay Specialty Polymers
Trade Name KetaSpire®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KetaSpire® KT-880P is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity and excellent chemical resistance to organics, acids and bases.These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing and other industrial uses. KetaSpire® KT-880P is intended for extrusion compounding. This powder is also available as KT-880NT in a natural-color pellet form for injection molding.Features: Ductile; Fatigue Resistant; Flame Retardant; Good Chemical Resistance; Good Dimensional Stability; Good Impact Resistance; High Flow; High Heat ResistanceUses: Electrical/Electronic Applications; Industrial Applications; Semiconductor Molding CompoundsInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ISO 62
Melt Flow 36 g/10 min

@Load 2.16 kg,
Temperature 400 °C
36 g/10 min

@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 100 MPa
14500 psi
ASTM D638
Elongation at Yield 5.2 %
5.2 %
ASTM D638
Tensile Modulus 3.80 GPa
551 ksi
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 3.90 GPa
566 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
27.8 µin/in-°F

@Temperature -58.0 - 122 °F
1
Melting Point 343 °C
649 °F
DSC
Deflection Temperature at 1.8 MPa (264 psi) 159 °C
318 °F
Unannealed; ASTM D648
Glass Transition Temp, Tg 147 °C
297 °F
DSC
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Natural
Form Powder
Processing Technique Compression Molding; Electrostatic Spray Coating
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: