Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Parmax® 1200 Self-Reinforcing Polyethersulfone  (discontinued **)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Parmax® 1200 Self-Reinforcing Polyethersulfone  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PARMAX 1200 self-reinforcing polymer (SRP) is an ultra-high performance amorphous, melt-processable engineering thermoplastic. The unique properties of this material are due primarily to the inherent rigid-rod structure. PARMAX SRP is differentiated from other thermoplastics by outstanding mechanical properties without fiber reinforcement, scratch resistance, great friction and wear properties, excellent solvent resistance, and exceptional low temperature performance.PARMAX 1200 SRP has great thermal and thermal-oxidative stability and it is noncombustible. The specific strength of PARMAX 1200 SRP exceeds many of the materials commonly encountered in structural applications. The resin also possesses excellent machinability permitting fabrication of parts such as fasteners to tolerances of less than one mil (0.025 mm). The excellent mechanical, chemical, thermal, and physical properties of PARMAX 1200 SRP make it the material of choice for a variety of applications including aircraft substructures, semiconductor components, bushings, bearings, and gears, light-weight vehicle suspensions systems, and medical tubing and other devices. PARMAX 1200 resin comes in natural or black pellets as extrusion grade – PARMAX 1200 EP (NT-001 and BK-002) and as Krum for compression molding – PARMAX 1200 CK (NT-001 and BK-002).Information provided by Solvay Advanced Polymers
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
Moisture Absorption at 24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.70 %
0.70 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell B 64
64
ASTM D785
Tensile Strength at Break 207 MPa
30000 psi
ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
ASTM D638
Flexural Strength 310 MPa
45000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Compressive Yield Strength 241 MPa
35000 psi
ASTM D695
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.7 J/cm
20.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear 30.6 µm/m-°C

@Temperature 20.0 °C
17.0 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ASTM D648
Glass Transition Temp, Tg 158 °C
316 °F
ASTM E 1356
Flammability, UL94 V-0
V-0
0.01 in.
Oxygen Index 49 %
49 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.1

@Frequency 1e+6 Hz
3.1

@Frequency 1e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Pencil Hardness 7H
ASTM D3363
Smoke Emission, Ds Max 1 at 1.5 min
ASTM E662
Max 1 at 4 min
ASTM E662