Solvay Specialty Polymers Polymist® XPP 515 Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Solvay Specialty Polymers
Trade Name Polymist®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Polymist® XPP 515 Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polymist® 515 a white PTFE micronized powder PTFE micronized powder composed of discrete particles. Designed for use in critical engineering and high end performance plastics applications, Polymist® XPP 515 will improve wear resistance and low coefficient of friction. Polymist® XPP 515 can also be used in elastomers to improve abrasion and tear resistance as well as non-stick properties, mar and abrasion resistance.Main features of Polymist® 515 are Improved wear resistance, Increased pressure x velocity (PV) limits, Reduced friction and stick-slip response, Improved lubricity, abrasion, scratch and rub resistance, Increased (hot) tear strengthUses: AdditiveAdditional Properties: Bulk Density - ASTM D4895 400 g/l; Melt Temperature - ASTM D3418 320 to 330 °C; Particle Size - Internal Method 20.0 µm; Specific Surface Area - Internal Method 3.0 m²/gInformation provided by Solvay Specialty Polymers.
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color White
Form Powder