Solvay Specialty Polymers Primef® 5084 30% GF PPS, Lubricated Grade  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Primef® 5084 30% GF PPS, Lubricated Grade  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Contains PTFE lubricant. Used for injection molding of high performance parts.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
Solvay Test Method
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 140 MPa
20300 psi
ISO 527
Elongation at Break 1.8 %
1.8 %
ISO 527
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527
Flexural Strength 190 MPa
27600 psi
ISO 178
Flexural Modulus 10.5 GPa
1520 ksi
ISO 178
Izod Impact, Notched 0.550 J/cm
1.03 ft-lb/in
ISO 180
Izod Impact, Unnotched 4.00 J/cm
7.49 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
Melting Point 280 °C
536 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ISO 75
Glass Transition Temp, Tg 90.0 °C
194 °F
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Processing Properties Metric English Comments
Nozzle Temperature 320 - 350 °C
608 - 662 °F
Melt Temperature 320 - 330 °C
608 - 626 °F
Mold Temperature 150 - 160 °C
302 - 320 °F
Copyright © lookpolymers.com All Rights Reserved