Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Manufacturer Solvay Specialty Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical Resistance; Good Electrical Properties; Good StrengthAdditional Properties: Heat Deflection Temperature - ASTM D648 265 °C; Insulation Resistance - (90°C): 1.00E+13 ohm; Mold Shrinkage - 0.20 %; Mold Shrinkage - 0.40 %; Temperature Index - UL 746B 220 to 240 °CInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ISO 1183
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength 150 MPa
21800 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Flexural Strength 230 MPa
33400 psi
ASTM D790
Flexural Modulus 18.0 GPa
2610 ksi
ISO 178
Compressive Strength 275 MPa
39900 psi
ASTM D695
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
Notch A; ISO 180
Izod Impact, Unnotched (ISO) 22.0 kJ/m²
10.5 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
2; ISO 11359-2
15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
2; ISO 11359-2
CTE, linear, Transverse to Flow 25.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
13.9 µin/in-°F

@Temperature -58.0 - 122 °F
ISO 11359-2
65.0 µm/m-°C

@Temperature 100 - 200 °C
36.1 µin/in-°F

@Temperature 212 - 392 °F
ISO 11359-2
Thermal Conductivity 0.640 W/m-K
4.44 BTU-in/hr-ft²-°F
ISO 8302
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
5VA

@Thickness 1.60 mm
5VA

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 5.0

@Frequency 1.00e+6 Hz
5.0

@Frequency 1.00e+6 Hz
ASTM D150
5.2

@Frequency 1000 Hz
5.2

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm
457 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 1000 Hz
0.0020

@Frequency 1000 Hz
ASTM D150
0.0020

@Frequency 1.00e+6 Hz
0.0020

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 185 sec
185 sec
ASTM D495
Comparative Tracking Index 250 V
250 V
UL 746
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
Latin America
North America
Color Natural
Form Pellets
RoHS Compliance RoHS Compliant