Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
Manufacturer Solvay Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Stability; High Impact ResistanceInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Filler Content 30 %
30 %
Glass Fiber
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 3.18 mm
0.0020 in/in

@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm

@Thickness 3.20 mm
0.0060 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 86
86
ASTM D785
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength 131 MPa
19000 psi
ASTM D638
Tensile Stress 135 MPa
19600 psi
ISO 527-2
Elongation at Break 2.0 %
2.0 %
ISO 527-2
2.0 %
2.0 %
ASTM D638
Flexural Strength 193 MPa
28000 psi
ASTM D790
200 MPa
29000 psi
ISO 178
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
9.00 GPa
1310 ksi
ISO 178
Compressive Strength 210 MPa
30500 psi
ASTM D695
Poissons Ratio 0.38
0.38
ASTM E132
Izod Impact, Notched 0.960 J/cm

@Thickness 3.18 mm
1.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 6.90 J/cm

@Thickness 3.18 mm
12.9 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Notched (ISO) 9.50 kJ/m²
4.52 ft-lb/in²
Notch A; ISO 180
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature 100 - 200 °C
5.56 µin/in-°F

@Temperature 212 - 392 °F
2
20.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
11.1 µin/in-°F

@Temperature -58.0 - 122 °F
2
CTE, linear, Transverse to Flow 55.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
30.6 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
90.0 µm/m-°C

@Temperature 100 - 200 °C
50.0 µin/in-°F

@Temperature 212 - 392 °F
TMA; ASTM E831
Thermal Conductivity 0.270 W/m-K
1.87 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 130 °C
266 °F
UL Temperature Rating
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Oxygen Index 34 %
34 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Insulation Resistance 1.00e+11 ohm

@Temperature 90.0 °C
1.00e+11 ohm

@Temperature 194 °F
IEC 60167
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
ASTM D150
3.8

@Frequency 1000 Hz
3.8

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm
559 kV/in
ASTM D149
Dissipation Factor 0.0030

@Frequency 1000 Hz
0.0030

@Frequency 1000 Hz
ASTM D150
0.0090

@Frequency 1.00e+6 Hz
0.0090

@Frequency 1.00e+6 Hz
ASTM D150
Arc Resistance 124 sec
124 sec
ASTM D495
Comparative Tracking Index 100 V
100 V
UL 746
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
Latin America
North America
Color Black
Form Pellets
RoHS Compliance RoHS Compliant