Solvay Specialty Polymers Tecnoflon® N 215 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Solvay Specialty Polymers
Trade Name Tecnoflon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Tecnoflon® N 215 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tecnoflon® N 215 is a very low viscosity fluoroelastomer copolymer. Tecnoflon® N 215 is intended for blending with other polymers of the Tecnoflon® family to achieve the desired viscosity. It is also intended for high concentration solution applications, such as dip coated items, fabric coatings and spray coating. Tecnoflon® N 215 can be mixed in the same way as all the other Tecnoflon® grades and can be used in any application requiring either very low compound viscosity or "low viscosity", highly loaded high hardness compounds. Tecnoflon® N 215 does not contain curatives: therefore the proper levels of Tecnoflon® FOR M1 and Tecnoflon® FOR M2 must be added to achieve the required properties. It can be also cured with diamine based systems such as Tecnoflon® Tecnocin A and Tecnoflon® Tecnocin B.Features: Copolymer; Good Adhesion; Good Flow; Low Compression Set; Low ViscosityUses: Blending; Coating Applications; Compounding; Fabric CoatingsAdditional Properties: Fluorine Content - 66 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Mooney Viscosity 10

@Temperature 121 °C
10

@Temperature 250 °F
ML 1+10; ASTM D1646
Descriptive Properties Value Comments
Availability Europe; North America
Color Translucent
Form Slab
Processing Technique Coating; Compounding; Dip Coating; Spraying