Solvay Specialty Polymers Torlon® 4000T Polyamide-imide (PAI)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyamide-imide (PAI) , Polyamide-Imide, Extruded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Torlon® 4000T Polyamide-imide (PAI)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Torlon 4000T is a neat resin polyamide-imide (PAI) coarse powder designed for compounding with other polymers and specialty additives. It is the base resin utilized in all Torlon injection molded compounds. Its powder form enables designers to enhance custom compounds and specialty applications with the well-known properties of Torlon polyamide-imide, from its unstoppable performance under extreme conditions to excellent resistance against wear, creep and chemicals. A fine-particle powder version, Torlon 4000TF, is also available, which is particularly well suited for compression molded parts. A water soluble analog of Torlon 4000T is available as Torlon AI-50. Torlon 4000T has been shown to be useful in blends with polyphenylsulfone (PPSU), polyethersulfone (PES), polysulfone (PSU), polyetheretherketone (PEEK), high-temperature sulfone resins, self-reinforced polyphenylene, polybenzimidizole (PBI), polyimide (PI), polyetherimide (PEI), and polyphenylene sulfide (PPS). Besides blending with other polymers to enhance properties, Torlon 4000T powder may be compounded with a wide variety of performance fillers, reinforcements, specialty additives and colorants to meet the desired need. The resultant compound may then be injection molded or extruded into film, shapes or fiber. In addition to molded components, Torlon PAI powders are suitable for use in other high performance forms. For example, these powders are soluble in dipolar aprotic solvents such as N-methyl pyrrolidone (NMP), dimethylacetamide (DMAC), dimethylsulfoxide (DMSO) and dimethylformamide (DMF). Solutions of these systems can be sprayed into coatings, cast into films, spun into fibers and cast or spun into specialty membranes. High strength, high temperature capable adhesives can be also formulated from Torlon PAI powders. Torlon PAI powders may be incorporated into epoxy and other thermoset systems to provide additional strength, ductility and heat resistance. Torlon 4000T powders are available in 3 viscosity grades, which are defined by the inherent viscosity (IV) ranges shown in the accompanying data. - Low viscosity: 4000T-LV - Medium viscosity: 4000T-MV - High viscosity: 4000T-HVInjection Notes: Drying Time/Temp: 4 hrs @ 300°F Drying Time/Temp: 16 hrs@ 250°FInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Viscosity Measurement 0.50 - 0.59

@Temperature 25.0 °C
0.50 - 0.59

@Temperature 77.0 °F
Torlon 4000T-LV, 0.5% in NMP; Intrinsic Viscosity
0.60 - 0.69

@Temperature 25.0 °C
0.60 - 0.69

@Temperature 77.0 °F
Torlon 4000T-MV, 0.5% in NMP; Intrinsic Viscosity
0.70 - 0.90

@Temperature 25.0 °C
0.70 - 0.90

@Temperature 77.0 °F
Torlon 4000T-HV, 0.5% in NMP; Intrinsic Viscosity
Processing Properties Metric English Comments
Drying Temperature 177 °C
351 °F
Dry Time 3.00 hour
3.00 hour
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Flame Retardant
Good Chemical Resistance
High Heat Resistance
Forms Powder
Generic PAI
Processing Method Coating
Compounding
Uses Blending
Cast Film
Coating Applications