Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyamide-imide (PAI) , Polyamide-Imide, Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Torlon 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon PAI grades cannot be molded successfully in molds with undercuts. Torlon 4601 has been formulated to be moldable in tools with minor undercuts and give very good performance in lubricated wear applications. Torlon PAI has the highest strength and stiffness of any thermoplastic up to 275°C (525°F). It has outstanding resistance to wear, creep, and chemicals. Potential applications for Torlon 4601 polyamide-imide include ball bearing cages and other molded articles that require undercut tooling.Injection Notes: Minimum drying times are: 3 hours at 350°F, 4 hours at 300°F, or 16 hours at 250°F. Compression Ratio: 1:1 to 1.5:1 Begin hold pressure at a high setting 6,000-8,000 psi (41.37-55.16 MPa), for several seconds, then drop off to 3,000-5,000 psi (20.69-34.48 MPa), for the duration of the hold pressure sequence. Molded parts must be cured.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 121 MPa
17500 psi
ASTM D638
Elongation at Break 4.1 %
4.1 %
ASTM D638
Tensile Modulus 4.21 GPa
611 ksi
ASTM D638
Flexural Strength 182 MPa
26400 psi
ASTM D790
Flexural Modulus 4.48 GPa
650 ksi
ASTM D790
Shear Strength 108 MPa
15700 psi
ASTM D732
Izod Impact, Notched 2.30 J/cm
4.31 ft-lb/in
ASTM D256
3.70 J/cm
6.93 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 284 °C
543 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 304 °C
579 °F
Nozzle Temperature 371 °C
700 °F
Mold Temperature 199 - 216 °C
390 - 421 °F
Drying Temperature 177 °C
351 °F
Dry Time 3.00 hour
3.00 hour
Moisture Content 0.050 %
0.050 %
Back Pressure 6.89 MPa
999 psi
Screw Speed 50 - 100 rpm
50 - 100 rpm
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Flame Retardant
Good Chemical Resistance
Good Creep Resistance
Good Wear Resistance
High Heat Resistance
High Temperature Strength
Forms Pellets
Generic PAI
Processing Method Injection Molding
Machining
Profile Extrusion
Screw L/D Ratio 18.0:1.0 to 24.0:1.0
Uses Bearings
Industrial Applications
Copyright © lookpolymers.com All Rights Reserved