Material Notes:
Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous hollow fiber and flat sheet membranes using a solvent-based process. These high molecular weight polymers are used in a variety of membrane filtration applications, such as renal dialysis, water treatment, bio-processing, food and beverage processing, and industrial gas separation. Udel polysulfone polymers possess a number of attributes that are valued by the membrane industry, including excellent mechanical properties, stability at pH levels from 2-13, excellent resistance to caustic and good resistance to moderate concentrations of chlorine. They feature low levels of extractible and insoluble materials making them suitable for drinking water and food contact uses. They may be sterilized using steam, ethylene oxide and e-beam radiation. Udel P-3500 LCD MB series polymers are available in various narrow molecular weight range grades, as shown below. Each grade features reduced levels of cyclic dimer compared to the previous grade, P-3500 NT 11. This can be important in solution processing applications such as membrane production, as it leads to improved dope solution stability and reduced equipment fouling. The Udel P-3500 LCD MB series polymers are soluble in commercially available, water-miscible, dipolar, aprotic solvents, such as dimethylacetamide (DMAC), dimethylformamide (DMF), and N-methylpyrrolidone (NMP). These materials offer membrane producers very good control of pore size and pore size distribution, high membrane strength, and good film-forming properties.Injection Notes: UDEL P-3500 polysulfones may be dried before preparing solutions. Pellets can be dried in a circulating hot air oven, by spreading the pellets on trays to a 1-2 inch depth and drying for 3.5 hours at 257 to 325°F (135 to 163°C).Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ASTM D570
Viscosity 2000 - 2800 cP

@Shear Rate 30.0 1/s,
Temperature 40.0 °C
2000 - 2800 cP

@Shear Rate 30.0 1/s,
Temperature 104 °F
P-3500 LCD MB7; 25 wt% polymer solution in DMAc
2200 - 3000 cP

@Shear Rate 30.0 1/s,
Temperature 40.0 °C
2200 - 3000 cP

@Shear Rate 30.0 1/s,
Temperature 104 °F
P-3500 LCD MB3; 25 wt% polymer solution in DMAc
2400 - 3200 cP

@Shear Rate 30.0 1/s,
Temperature 40.0 °C
2400 - 3200 cP

@Shear Rate 30.0 1/s,
Temperature 104 °F
P-3500 LCD MB8; 25 wt% polymer solution in DMAc
Molecular Weight 77000 - 83000 g/mol
77000 - 83000 g/mol
P-3500 LCD MB7
78000 - 84000 g/mol
78000 - 84000 g/mol
P-3500 LCD MB3
80000 - 86000 g/mol
80000 - 86000 g/mol
P-3500 LCD MB8
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.3 MPa
10200 psi
ASTM D638
Elongation at Break 50 - 100 %
50 - 100 %
ASTM D638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D638
Flexural Strength 106 MPa
15400 psi
ASTM D790
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Tensile Impact Strength 420 kJ/m²
200 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 174 °C
345 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+16 ohm-cm
3.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.02

@Frequency 1.00e+6 Hz
3.02

@Frequency 1.00e+6 Hz
ASTM D150
3.03

@Frequency 60.0 Hz
3.03

@Frequency 60.0 Hz
ASTM D150
3.04

@Frequency 1000 Hz
3.04

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
ASTM D150
0.0060

@Frequency 1.00e+6 Hz
0.0060

@Frequency 1.00e+6 Hz
ASTM D150
0.0070

@Frequency 60.0 Hz
0.0070

@Frequency 60.0 Hz
ASTM D150
Processing Properties Metric English Comments
Zone 1 302 °C
576 °F
Zone 5 316 - 338 °C
601 - 640 °F
Melt Temperature 316 - 371 °C
601 - 700 °F
Drying Temperature 135 - 163 °C
275 - 325 °F
Dry Time 3.50 hour
3.50 hour
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1655
NSF Unspecified Rating
Appearance Natural Color
Availability Asia Pacific
Europe
North America
South America
Features Acid Resistant
Alcohol Resistant
Alkali Resistant
Good Chemical Resistance
Good Toughness
High Heat Resistance
Hydrocarbon Resistant
Hydrolytically Stable
Forms Pellets
Generic PSU
Processing Method Cast Film
Injection Molding
Solution Processing
RoHS Compliance RoHS Compliant
Uses Membranes