Material Notes:
Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. The advantages of Udel P-3500 LCD are attributed to the lower level of cyclic dimer present in the polymer. Polysulfone is a tough, rigid and transparent high-strength thermoplastic that is suitable for long-term use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstands prolonged exposure to high temperatures and repeated sterilization. Polysulfone is resistant to mineral acids, alkali, salt solutions, detergents and hydrocarbon oils. Contact with polar solvents such as ketones, chlorinated hydrocarbons and aromatic hydrocarbons should be avoided, as these types of chemical compounds can cause stress cracking or solvate polysulfone resin. Polysulfone is highly resistant to degradation by gamma or electron beam radiation but can be adversely affected by long term exposure to ultraviolet. Electrical properties of the polymer are very stable over a wide range of temperatures and after immersion in water or exposure to high humidity. The resin is very safe for food contact uses. It complies with FDA 21 CFR 177, 1655 and may be used in articles intended for repeated use in contact with foods. Additionally, it is approved by the NSF, by the Department of Agriculture for contact with meat and poultry and the 3-A Sanitary Standards of the Dairy Association. - Transparent: Udel P-3500 NT LCDInjection Notes: UDEL P-3500 polysulfones may be dried before preparing solutions. Pellets can be dried in a circulating hot air oven, by spreading the pellets on trays to a 1-2 inch depth and drying for 3.5 hours at 257 to 325°F (135 to 163°C).Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Water Absorption 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ASTM D955
Melt Flow 3.0 - 5.0 g/10 min

@Load 2.16 kg,
Temperature 343 °C
3.0 - 5.0 g/10 min

@Load 4.76 lb,
Temperature 649 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.3 MPa
10200 psi
ASTM D638
Elongation at Break 50 - 100 %
50 - 100 %
ASTM D638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D638
Flexural Strength 106 MPa
15400 psi
ASTM D790
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm
1.29 ft-lb/in
ASTM D256
Tensile Impact Strength 420 kJ/m²
200 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
31.1 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 174 °C
345 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+16 ohm-cm
3.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.02

@Frequency 1.00e+6 Hz
3.02

@Frequency 1.00e+6 Hz
ASTM D150
3.03

@Frequency 60.0 Hz
3.03

@Frequency 60.0 Hz
ASTM D150
3.04

@Frequency 1000 Hz
3.04

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
ASTM D150
0.0060

@Frequency 1.00e+6 Hz
0.0060

@Frequency 1.00e+6 Hz
ASTM D150
0.0070

@Frequency 60.0 Hz
0.0070

@Frequency 60.0 Hz
ASTM D150
Processing Properties Metric English Comments
Zone 1 302 °C
576 °F
Zone 5 316 - 338 °C
601 - 640 °F
Melt Temperature 316 - 371 °C
601 - 700 °F
Drying Temperature 135 - 163 °C
275 - 325 °F
Dry Time 3.50 hour
3.50 hour
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1655
NSF 61
Tested at 82 °C (180 °F) (Commercial Hot)
Appearance Natural Color
Availability Asia Pacific
Europe
North America
South America
Features Acid Resistant
Alcohol Resistant
Alkali Resistant
Detergent Resistant
Good Chemical Resistance
Good Dimensional Stability
Good Sterilizability
Good Surface Finish
Good Toughness
High Heat Resistance
Hydrocarbon Resistant
Hydrolytically Stable
Steam Sterilizable
Forms Pellets
Generic PSU
Processing Method Extrusion
Extrusion Blow Molding
Film Extrusion
Injection Blow Molding
Injection Molding
Machining
Pipe Extrusion
Profile Extrusion
Sheet Extrusion
Thermoforming
RoHS Compliance RoHS Compliant
Uses Membranes
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved