Solvay Specialty Polymers Veradel® 3300 Polyethersulfone (PESU)  (discontinued **)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Veradel® 3300 Polyethersulfone (PESU)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Veradel 3300 polyethersulfone (PESU) is a medium melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. Other desirable properties include thermal stability, creep resistance and inherent flame resistance. Veradel 3300 is suggested for general purpose injection molding. Three other grades are available: Veradel 3200, a low melt flow grade that can be processed by extrusion or injection molding; Veradel 3400, a high melt flow grade designed for easy molding of parts with thin walls or long flow lengths and Veradel 3600, a very high melt flow grade suggested for compounding, especially of glass or carbon fiber reinforced compounds.This grade was formerly marketed as Gafone™ PESUFeatures: Acid Resistant; Flame Retardant; General Purpose; Good Adhesion; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight; Medium RigidityUses: Appliance Components; Appliances; Automotive Electronics; Batteries; Business Equipment; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; General Purpose; Industrial Applications; Microwave CookwareAvailability: Africa & Middle East; Asia Pacific; Europe; North America; South AmericaInformation provide by Solvay Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Water Absorption 0.50 %
0.50 %
24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 380 °C
30 g/10 min

@Load 4.76 lb,
Temperature 716 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Elongation at Yield 6.5 %
6.5 %
ASTM D638
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Flexural Strength 125 MPa
18100 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 52.0 µm/m-°C
28.9 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
Annealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.70e+15 ohm-cm
1.70e+15 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1000 Hz
3.5

@Frequency 1000 Hz
ASTM D150
3.51

@Frequency 60.0 Hz
3.51

@Frequency 60.0 Hz
ASTM D150
3.54

@Frequency 1.00e+6 Hz
3.54

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
381 kV/in
ASTM D149
Dissipation Factor 0.0017

@Frequency 60.0 Hz
0.0017

@Frequency 60.0 Hz
ASTM D150
0.0022

@Frequency 1000 Hz
0.0022

@Frequency 1000 Hz
ASTM D150
0.0056

@Frequency 1.00e+6 Hz
0.0056

@Frequency 1.00e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Melt Temperature 343 - 385 °C
649 - 725 °F
Mold Temperature 149 - 163 °C
300 - 325 °F
Drying Temperature 177 °C
351 °F
Dry Time 2.50 hour
2.50 hour
Descriptive Properties Value Comments
Additional Properties Water Absorption - ASTM D570: 1.9 %
Agency Ratings NSF 61
Appearance Transparent - Slight Yellow
Forms Pellets
Injection Rate Fast
Processing Method Compounding
Injection Molding
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.0:1.0