Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU), 20% Glass Fiber

Category Polymer , Thermoplastic , Polyethersulfone (PES) , Polyethersulfone (PES), 20%Glass Fiber Filled
Manufacturer Solvay Specialty Polymers
Trade Name Veradel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU), 20% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Veradel® AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resistance of the material, while maintaining most of its other basic characteristics. The combination of structural properties and cost effectiveness make this resin an attractive alternative to metals in many engineering applications.Features: Acid Resistant; Flame Retardant; Food Contact Acceptable; Good Adhesion; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Strength; Good Thermal Stability; Good Toughness; High Heat Resistance; High Rigidity; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular WeightUses: Appliance Components; Appliances; Automotive Electronics; Batteries; Business Equipment; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Industrial Applications; Metal Replacement; Microwave Cookware; Plumbing Parts; Valves/Valve PartsAutomotive Specifications FORD WSK-M4D773-A2 Color: BK184 Black; FORD WSK-M4D773-A2 Color: NT NaturalInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Filler Content 20 %
20 %
Glass Fiber
Water Absorption 0.45 %

@Time 86400 sec
0.45 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 343 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 649 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 109 MPa
15800 psi
ASTM D638
Elongation at Break 3.2 %
3.2 %
ASTM D638
Tensile Modulus 5.69 GPa
825 ksi
ASTM D638
Flexural Strength 162 MPa
23500 psi
ASTM D790
Flexural Modulus 6.55 GPa
950 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm
1.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Thickness 3.18 mm
17.2 µin/in-°F

@Thickness 0.125 in
Deflection Temperature at 1.8 MPa (264 psi) 214 °C

@Thickness 3.20 mm
417 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 0.787 mm
V-0

@Thickness 0.0310 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.84

@Frequency 60.0 Hz
3.84

@Frequency 60.0 Hz
ASTM D150
3.84

@Frequency 1000 Hz
3.84

@Frequency 1000 Hz
ASTM D150
3.88

@Frequency 1.00e+6 Hz
3.88

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Dissipation Factor 0.0015

@Frequency 60.0 Hz
0.0015

@Frequency 60.0 Hz
ASTM D150
0.0018

@Frequency 1000 Hz
0.0018

@Frequency 1000 Hz
ASTM D150
0.0081

@Frequency 1.00e+6 Hz
0.0081

@Frequency 1.00e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
NSF Yes
Yes
NSF 51
Processing Properties Metric English Comments
Melt Temperature 343 - 399 °C
649 - 750 °F
Mold Temperature 149 - 163 °C
300 - 325 °F
Drying Temperature 149 - 177 °C

@Time 9000 - 14400 sec
300 - 351 °F

@Time 2.50 - 4.00 hour
Back Pressure 0.345 - 0.689 MPa
50.0 - 99.9 psi
Descriptive Properties Value Comments
Agency Ratings NSF 51
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Colors Available; Natural
Form Pellets
Injection Rate Fast
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.0:1.0