Solvay TECHNYL® 27010ST PA66, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® 27010ST PA66, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2710ST is used in all sector of industry, offering an excellent productivity. This grade is widely used for: Sports and leisure applications for shoe soles, ski components, ski and surf bindings; Toy applications, such as, the bumper of a remote-controlled car and Battery gaskets, Fastener. This product is available in available in natural, black and in colors on request.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC60250
Dielectric Strength 16.0 kV/mm
406 kV/in
IEC 60243
Dissipation Factor 0.060
0.060
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Copyright © lookpolymers.com All Rights Reserved