Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218 V30 BK 34 NG-K PA66, 33% glass fiber, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 218 V30 Black 34 NG-K is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This product has been specially designed to improve its resistance to automotive cooling liquids, increasing lifetime of parts in permanent contact with such a liquid.Available in: Asia Pacific Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applicationsApplications: Cooling and heating radiator systems, header tanks, thermostat components, inlet & outlet pipes…Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183/A
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
Mechanical Properties Metric English Comments
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Strength 290 MPa
42100 psi
ASTM D790
Flexural Modulus 9.50 GPa
1380 ksi
ASTM D790
Izod Impact, Notched 1.15 J/cm
2.15 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
13.9 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
CTE, linear, Transverse to Flow 2.50 µm/m-°C

@Temperature 23.0 - 85.0 °C
1.39 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 262 °C
504 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ISO 75/Af
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
1210
Oxygen Index 23 %
23 %
ISO 4589
Glow Wire Test 650 °C

@Thickness 1.60 mm
1200 °F

@Thickness 0.0630 in
Ignition Temperature; ISO 60695-2-13
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 6.00e+14 ohm
6.00e+14 ohm
IEC 60093
Dielectric Constant 3.7
3.7
IEC 60250
Dielectric Strength 34.0 kV/mm
864 kV/in
IEC 60243
Dissipation Factor 0.010
0.010
IEC 60250
Comparative Tracking Index 350 V
350 V
Solution B; IEC 60112
450 V
450 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 260 - 270 °C
500 - 518 °F
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 270-280°C
Mixing Zone 280-290°C