Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This product has been specially designed to improve its resistance to automotive cooling liquids, increasing lifetime of parts in permanent contact with such a liquids.Available in: Asia Pacific, Europe, Latin America and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: Cooling and heating radiator systems, header tanks, thermostat components, inlet & outlet pipes...Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
ISO 527 Type 1A
Tensile Stress 25.0 MPa

@Strain 1.00 %,
Temperature 150 °C
3630 psi

@Strain 1.00 %,
Temperature 302 °F
30.0 MPa

@Strain 1.00 %,
Temperature 120 °C
4350 psi

@Strain 1.00 %,
Temperature 248 °F
40.0 MPa

@Strain 1.00 %,
Temperature 80.0 °C
5800 psi

@Strain 1.00 %,
Temperature 176 °F
40.0 MPa

@Strain 2.00 %,
Temperature 150 °C
5800 psi

@Strain 2.00 %,
Temperature 302 °F
50.0 MPa

@Strain 2.00 %,
Temperature 120 °C
7250 psi

@Strain 2.00 %,
Temperature 248 °F
50.0 MPa

@Strain 3.00 %,
Temperature 150 °C
7250 psi

@Strain 3.00 %,
Temperature 302 °F
55.0 MPa

@Strain 1.00 %,
Temperature 23.0 °C
7980 psi

@Strain 1.00 %,
Temperature 73.4 °F
55.0 MPa

@Strain 4.00 %,
Temperature 150 °C
7980 psi

@Strain 4.00 %,
Temperature 302 °F
60.0 MPa

@Strain 3.00 %,
Temperature 120 °C
8700 psi

@Strain 3.00 %,
Temperature 248 °F
65.0 MPa

@Strain 4.00 %,
Temperature 120 °C
9430 psi

@Strain 4.00 %,
Temperature 248 °F
65.0 MPa

@Strain 8.00 %,
Temperature 150 °C
9430 psi

@Strain 8.00 %,
Temperature 302 °F
70.0 MPa

@Strain 2.00 %,
Temperature 80.0 °C
10200 psi

@Strain 2.00 %,
Temperature 176 °F
70.0 MPa

@Strain 8.00 %,
Temperature 120 °C
10200 psi

@Strain 8.00 %,
Temperature 248 °F
75.0 MPa

@Strain 1.00 %,
Temperature 0.000 °C
10900 psi

@Strain 1.00 %,
Temperature 32.0 °F
75.0 MPa

@Strain 3.00 %,
Temperature 80.0 °C
10900 psi

@Strain 3.00 %,
Temperature 176 °F
80.0 MPa

@Strain 4.00 %,
Temperature 80.0 °C
11600 psi

@Strain 4.00 %,
Temperature 176 °F
80.0 MPa

@Strain 8.00 %,
Temperature 80.0 °C
11600 psi

@Strain 8.00 %,
Temperature 176 °F
95.0 MPa

@Strain 2.00 %,
Temperature 23.0 °C
13800 psi

@Strain 2.00 %,
Temperature 73.4 °F
100 MPa

@Strain 1.00 %,
Temperature -40.0 °C
14500 psi

@Strain 1.00 %,
Temperature -40.0 °F
110 MPa

@Strain 3.00 %,
Temperature 23.0 °C
16000 psi

@Strain 3.00 %,
Temperature 73.4 °F
115 MPa

@Strain 4.00 %,
Temperature 23.0 °C
16700 psi

@Strain 4.00 %,
Temperature 73.4 °F
135 MPa

@Strain 2.00 %,
Temperature 0.000 °C
19600 psi

@Strain 2.00 %,
Temperature 32.0 °F
150 MPa

@Strain 3.00 %,
Temperature 0.000 °C
21800 psi

@Strain 3.00 %,
Temperature 32.0 °F
155 MPa

@Strain 4.00 %,
Temperature 0.000 °C
22500 psi

@Strain 4.00 %,
Temperature 32.0 °F
175 MPa

@Strain 2.00 %,
Temperature -40.0 °C
25400 psi

@Strain 2.00 %,
Temperature -40.0 °F
Tensile Modulus 7.50 GPa
1090 ksi
ISO 527 Type 1A
Flexural Strength 185 MPa
26800 psi
ISO 178
Flexural Modulus 6.40 GPa
928 ksi
ISO 178
Izod Impact, Unnotched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 8.80 J/cm²
41.9 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 29.0 kV/mm
737 kV/in
IEC 60243
Dissipation Factor 0.11
0.11
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %