Material Notes:
Description: Unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for very fast cycles.Available in: Europe, Latin America and North AmericaProduct Applications: TECHNYL ® A 225F offers two main advantages excellent filling qualities and UL 94 V2 under 0.4 mm. It is particularly used in electrical applications to mould parts with a good dimensional stability, such as: Unfilled bobbin coil forers for electrical motors, Transformers, and Connectors. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527 Type 1A
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527 type 1 A
Elongation at Break 100 %
100 %
ISO 527 Type 1A
Elongation at Yield 25 %
25 %
ISO 527 type 1 A
Tensile Modulus 2.00 GPa
290 ksi
ISO 527 Type 1A
Flexural Strength 55.0 MPa
7980 psi
ISO 178
Flexural Modulus 1.40 GPa
203 ksi
ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 4.00e+11 ohm
4.00e+11 ohm
IEC 60093
Dielectric Constant 3.2
3.2
IEC 60250
Dielectric Strength 226 kV/mm
5740 kV/in
IEC 60243
Dissipation Factor 0.080
0.080
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %