Material Notes:
Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 246M offers an excellent notched impact resistance at low temperature make it suitable for: sports and leisure applications, for shoe soles, ski components, ski and surf bindings, toy applications, such as, the bumper of a remote-controlled car. This product is available in natural, white and black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
ISO 527 Type 1A
Tensile Modulus 0.600 GPa
87.0 ksi
ISO 527 Type 1A
Flexural Strength 27.0 MPa
3920 psi
ISO 178
Flexural Modulus 0.700 GPa
102 ksi
ISO 178
Izod Impact, Notched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 10.0 J/cm²
47.6 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 4.00 kV/mm
102 kV/in
IEC 60243
Dissipation Factor 0.060
0.060
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %