Solvay TECHNYL® C 218 V40 PA6, 40% glass fiber, Eh 0

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 218 V40 PA6, 40% glass fiber, Eh 0.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL C 218 V40 is a polyamide 6 with 40% of glass fiber and with thermal stability.Colors: it is marketed in the black color and natural.Available in: Latin AmericaMain Properties: ? Good thermal resistance, ?Excellent dimensional stability, Good impact resistance. Applications: TECHNYL C 218 V40 was developed for applications on parts where good mechanical properties as impact resistance, superficial aspect and dimensional stability are required.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183/A
Water Absorption 0.90 %

@Temperature 23.0 °C,
Time 86400 sec
0.90 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 210 MPa
30500 psi
ISO R 527
Elongation at Break 2.3 %
2.3 %
ISO R 527
Tensile Modulus 13.1 GPa
1900 ksi
ISO R 527
Izod Impact, Notched (ISO) 16.0 kJ/m²
7.61 ft-lb/in²
ISO 180
Charpy Impact Unnotched 10.7 J/cm²
50.9 ft-lb/in²
ISO 179
Charpy Impact, Notched 1.80 J/cm²
8.57 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
Deflection Temperature at 1.8 MPa (264 psi) 214 °C
417 °F
ISO 75/Af
Flammability, UL94 HB
HB
Oxygen Index 23 %
23 %
ISO 4589
Glow Wire Test 650 °C

@Thickness 1.60 mm
1200 °F

@Thickness 0.0630 in
CEI 695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 93
Dielectric Constant 3.8
3.8
CEI 250
Dissipation Factor 0.020
0.020
CEI 250
Comparative Tracking Index 550 V
550 V
CEI 112
Processing Properties Metric English Comments
Feed Temperature 240 - 260 °C
464 - 500 °F
Nozzle Temperature 230 - 240 °C
446 - 464 °F
Mold Temperature 80.0 - 100 °C
176 - 212 °F
Descriptive Properties Value Comments
Compression Zone 230-240°C
Mixing Zone 240-250°C