Material Notes:
Description: Unreinforced polyamide PA6, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: This grade has improved impact strength and higher flexibility. It is suitable specially to make technical parts having small or medium size, such as: plugs, seals. This product is available in colors on request.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.0 MPa
5660 psi
ISO 527 type 1 A
Tensile Modulus 1.00 GPa
145 ksi
ISO 527 Type 1A
Flexural Strength 35.0 MPa
5080 psi
ISO 178
Flexural Modulus 0.800 GPa
116 ksi
ISO 178
Izod Impact, Notched (ISO) 82.0 kJ/m²
39.0 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 9.00 J/cm²
42.8 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 18.0 kV/mm
457 kV/in
IEC 60243
Dissipation Factor 0.12
0.12
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %