Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This grade has good mechanical properties, flame retardant rating UL94 V0 and glow-wire at 960°C. It is specially suitable for pieces such as: switches, timers, etc. This product is available in Natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
ISO 527 Type 1A
Elongation at Break 6.0 %
6.0 %
ISO 527 Type 1A
Tensile Modulus 8.05 GPa
1170 ksi
ISO 527 Type 1A
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Dielectric Strength 38.0 kV/mm
965 kV/in
IEC 60243
Dissipation Factor 0.060
0.060
IEC 60250
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following: