Material Notes:
Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled partsAvailable in: Asia Pacific, Europe, Latin America and North America Product Applications: This grade is Halogen and Red Phosphorous free fire resistant flame retardant grade is particularly suitable for equipment requiring robust glow-wire resistance with excellent molding and electrical performance, such as for MCB housings, contactors and switches and sockets. This grade is available in Grey, White, Natural and Black colors. Laser marking grades and other colors are available upon request.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527 Type 1A
Elongation at Break 4.8 %
4.8 %
ISO 527 Type 1A
Tensile Modulus 4.55 GPa
660 ksi
ISO 527 Type 1A
Charpy Impact Unnotched 7.90 J/cm²
37.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.340 J/cm²

@Temperature -30.0 °C
1.62 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
0.860 J/cm²

@Temperature 23.0 °C
4.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Electrical Properties Metric English Comments
Dielectric Strength 27.0 kV/mm
686 kV/in
IEC 60243
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %