Solvay TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 610 , Nylon 610, Glass Reinforced
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® eXten D 218 V30 is a 30% Glass Fiber reinforced and heat stabilized product suitable to the manufacturing of all injection molded parts. This material is available in black.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: TECHNYL® eXten D 218 V30 is suitable to the manufacturing of injection molded parts in all sectors of applications. It offers excellent chemical resistance, low water absorption, very good mechanical properties and mold ability.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 112 MPa
16200 psi
ISO 527 Type 1A
Elongation at Break 7.5 %
7.5 %
ISO 527 Type 1A
Tensile Modulus 6.10 GPa
885 ksi
ISO 527 Type 1A
Flexural Strength 193 MPa
28000 psi
ISO 178
Flexural Modulus 6.10 GPa
885 ksi
ISO 178
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %