Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is available in black and natural colors.Benefits: Due to its outstanding flow characteristics, the product shows exceptional processing behavior and excellent surface aspect of the finished part.Available in: Europe, Latin America and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: The product is particularly suitable for all applications where a high rigidity is required: typically structural parts or brackets for the automotive industry. Its high mechanical performance allows that product to be an alternative to metal parts.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 180 MPa
26100 psi
ISO 527 Type 1A
Elongation at Break 3.5 %
3.5 %
ISO 527 Type 1A
Tensile Modulus 12.5 GPa
1810 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 91.0 kJ/m²
43.3 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 10.4 J/cm²
49.5 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 2.10 J/cm²
9.99 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %