Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaProduct Applications: Due to its outstanding flow characteristics, TECHNYLSTAR TM S 216 V30 provides a significant productivity improvement and allows more freedom in mould design and part design versus standard polyamide solutions. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
16000 psi
ISO 527 Type 1A
Elongation at Break 5.5 %
5.5 %
ISO 527 Type 1A
Tensile Modulus 6.20 GPa
899 ksi
ISO 527 Type 1A
Flexural Modulus 5.20 GPa
754 ksi
ISO 178
Izod Impact, Notched (ISO) 19.0 kJ/m²
9.04 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 65.0 kJ/m²
30.9 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.41 J/cm²
6.71 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 4.5
4.5
IEC 60250
Dielectric Strength 22.0 kV/mm
559 kV/in
IEC 60243
Dissipation Factor 0.090
0.090
IEC 60250
Comparative Tracking Index 475 V
475 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %